GH3652 pipes and tubing are available in a variety of forms and sizes:
Forms: Seamless pipes/tubing are available.

Outer Diameter (OD): Typically ranges from 1/8 inch to 48 inches (seamless pipes can be up to 26 inches).
Wall Thickness: Available in various wall thickness grades (e.g., SCH 20 to SCH 160, XXS) or specific wall thicknesses (e.g., 0.5 mm to 50 mm).
Heat Treatment: Available in various heat treatment states, including annealing, solution treatment, and aging, or quenched and tempered (Q+T).
Αποστολή ερώτησής
Chat τώρα

Ως κορυφαίος προμηθευτής και κατασκευαστής στην Κίνα, η GNEE Steel παρέχει οικονομικά-προϊόντα από κράμα με βάση το νικέλιο-.

Εισαγωγή προϊόντος

GH3652 high-temperature alloy steel pipes for chemical processing plants description

GH1016 high-temperature alloy steel pipe for gas turbine engines

GNEE GH3652 high-temperature alloy steel pipes for chemical processing plants

 

GH3652 is a high-quality nickel-based high-temperature alloy pipe widely used in chemical processing plants due to its superior performance under extreme conditions. It is specifically designed to withstand high-temperature and corrosive environments, where ordinary stainless steel or carbon steel would fail.

 

Specification Of GH3652 high-temperature alloy steel pipes for chemical processing plants

 

GH3652 Range of products

0.08-200mm(T)*W*L Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Φ8-1200mm*L
0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
OD:6-219mm x WT:0.5-20.0mm Annealed, Solution and Aging, Q+T, ACID-WASHED

 

GH3652 high-temperature alloy steel pipes for chemical processing plants Specification

 

GH3652 high-temperature alloy steel pipe Chemical composition(mass fraction)(wt.%)

Min.(>=) Max.(<=)
C - 0.1
26.5 28.5
-
2.8 3.5
- 1
- 0.03
- 0.8
- 0.3
P - 0.02
S - 0.02

 

Mechanical properties of grade GH3652 Tube

As-Heat-Treated Condition
Rp0.2(MPa) R A(%) Z(%)
556 (>=) 963 (>=) 43 34 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 241

 

Physical properties of grade GH3652 Pipe

kg/dm3 kN/mm2
899 (>=) 655 (>=) 33 21 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 241
Temp.

 

 

 

 

 

(10000h) (10000h)

 

(Rp1,0) N/mm2 (Rp1,0) N/mm2
396 638 761

 

 

 

Features Of GH3652 high-temperature alloy steel pipes for chemical processing plants

 

GH3652 High-Temperature Alloy Steel Pipes For Chemical Processing Plants

Applications of GH3652 Pipes in Chemical Processing Plants

GH3652 alloy pipes are widely used in critical high-stress areas of chemical processing plants, including:

Reactors and Boilers: Components subjected to extreme high temperatures and pressures.

Heat Exchangers: Suitable for equipment requiring efficient heat transfer under corrosive and high-temperature conditions.

High-Pressure Piping Systems: Essential equipment for transporting high-temperature fluids and gases in processes such as oil refining and petrochemical production.

Furnaces and Industrial Equipment: Used in other high-temperature industrial furnaces and power generation equipment where conventional materials cannot meet the requirements.

 

GH3652 high-temperature alloy steel pipes for chemical processing plants Surface Treatments

  • Pickling treatment
  • Mirror polishing treatment
  • Polishing treatment
  • Sandblasting treatment

Gnee Steel provides four surface treatments for GH3652 high-temperature alloy steel pipes for chemical processing plants: pickling, mirror polishing, polishing, and sandblasting.

 

GH3652 high-temperature alloy steel pipes for chemical processing plants production process

  • Annealing process
  • Hot rolling process
  • Cold drawing process
  • Solution + aging process
    Solution + aging process

Gnee Steel provides the following heat treatments for GH3652 high-temperature alloy steel pipes for chemical processing plants: annealing, solution + aging. In addition, Gnee Steel also provides hot working and cold working, which are hot rolling and cold drawing.

 

GH3652 high-temperature alloy steel pipes for chemical processing plants Packaging 

  • Steel strapping
  • Wooden boxes/crates
  • Rainproof cloth packaging
  • Airworthy export packaging 

     

     

In order to better ensure the safety of your goods, we will provide professional, environmentally friendly, convenient and efficient packaging services.

 

 

Gnee Steel

 

Gnee Steel specializes in the production and sale of various nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy Alloy 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, and high-temperature alloys. Gnee Steel's products are widely used in aerospace, chemical, electric power, automotive, and nuclear energy applications. We also offer customized alloy solutions tailored to customer needs. For alloy pricing inquiries or customized alloy solutions, please contact us for a quote at ss@gneesteel.com.

Q:What is the delivery time for Waspaloy GH4738 thin-walled tubes?

A: Approximately 7-20 days, depending on the quantity of Waspaloy GH4738 thin-walled tubes and production status.

Q:What kind of packaging is used for Waspaloy GH4738 thin-walled tubes?

A: Usually, we use cartons or plywood boxes, filled with protective material to ensure the safety of the Waspaloy GH4738 thin-walled tubes.

Q:What is the lead time for Waspaloy GH4738 thin-walled tubes?

A: It takes approximately 10-25 days from order placement to receipt.